Standard and edition
Confirm the controlling document; a grade name or cross-reference alone is not a complete acceptance specification.
Stainless Steel Round Bar | Duplex Steel Round Bar | High Nickel Alloy Round Bar
Duplex Steel Round Bar
UNS S31803 is a duplex stainless steel grade with a combined ferritic and austenitic structure. It offers high yield strength and good resistance to pitting, crevice corrosion and chloride stress corrosion cracking in suitable service conditions.
This grade belongs to the 2205 family, but its chemistry limits differ from UNS S32205. When ordering round bar, specify UNS S31803, the material standard, diameter, length, solution-annealed condition and inspection documents.

At a glance
Confirm the applicable specification and availability for your required size and condition.
Buyer selection guide
Begin with the drawing, equipment specification, or governing code. The product name identifies the material route; acceptance depends on the complete purchase specification.
Common applications
UNS S31803 round bars are used for machined parts that need both strength and corrosion resistance. Suitability must be checked against operating temperature, chlorides, loads and the governing design requirements.
Compare the duplex round bar range and super duplex round bars when higher localized-corrosion resistance is being considered.
Specifications
Specify the exact UNS grade and product standard for acceptance. The name 2205 alone does not establish the certified chemical limits or bar condition.
| Requirement | Information |
|---|---|
| Material grade | UNS S31803 duplex stainless steel (2205 family) |
| European reference | EN 1.4462 / X2CrNiMoN22-5-3 (confirm applicable standard) |
| General bar specification | ASTM A276/A276M, where applicable |
| Pressure-service bar specification | ASTM A479/A479M, where applicable |
| Condition | Solution annealed and cooled as required by the product specification |
| Dimensions | Diameter, length, straightness and dimensional tolerance as ordered |
| Surface finish | Hot finished, peeled, turned or ground, subject to availability |
| Inspection | Mill test certificate with heat number, chemical and mechanical results; additional tests as specified |
For exact dimensional tolerance, specify the tolerance class and diameter on the purchase order. The incomplete ISO tolerance chart in the original page has been removed to avoid misleading values.
For related finishes see bright round bars and forged bars.
Chemical composition
These are widely referenced chemical-composition limits for UNS S31803, in percent by mass. The exact requirement is controlled by the specified standard and edition. Do not substitute the narrower UNS S32205 chemistry limits.
| Element | UNS S31803 (wt. %) |
|---|---|
| Chromium (Cr) | 21.0–23.0 |
| Nickel (Ni) | 4.50–6.50 |
| Molybdenum (Mo) | 2.50–3.50 |
| Nitrogen (N) | 0.08–0.20 |
| Carbon (C) | 0.030 maximum |
| Manganese (Mn) | 2.00 maximum |
| Silicon (Si) | 1.00 maximum |
| Phosphorus (P) | 0.030 maximum |
| Sulfur (S) | 0.020 maximum |
| Iron (Fe) | Balance |
Confirm actual chemistry and heat identification using the mill test certificate.
Mechanical properties
The following are reference requirements for solution-annealed UNS S31803 bars in published ASTM A276 editions. Bar size, processing and the applicable standard edition must be checked before acceptance.
| Property | Published reference value |
|---|---|
| Minimum tensile strength | 620 MPa (90 ksi) |
| Minimum 0.2% yield strength | 448 MPa (65 ksi) |
| Minimum elongation | 25% |
| Maximum Brinell hardness | 290 HB (published ASTM A276 reference) |
| Supply condition | Solution annealed |
| Magnetic behaviour | Normally magnetic due to ferrite content |
These values are not a substitute for the controlling purchase specification and certified test results. Other standards may round 448 MPa to 450 MPa.
Technical considerations
Confirm the controlling document; a grade name or cross-reference alone is not a complete acceptance specification.
Check that property values apply to the required diameter, heat treatment, test direction and temperature.
State tolerances, straightness, length, surface finish, machining allowance, and end condition where required.
Define inspection, test reports, marking, heat identification, third-party requirements, and destination documentation.
Grade designations
| Designation | Relationship |
|---|---|
| UNS S31803 | Specified grade on this page |
| Duplex 2205 | Common duplex grade family name |
| EN 1.4462 | Related European designation; verify the selected edition |
| SAF 2205 | Commercial name used within the duplex 2205 family |
| UNS S32205 | Related grade with tighter chemistry requirements; not automatically interchangeable |
Compare UNS S32205 round bar and SAF 2205 round bar for project-specific grade selection.
More about the material
Hot-finished bars may require extra machining allowance for final diameter and finish. Peeled, turned or ground products can reduce preparation work when tighter tolerances are needed. Confirm the supplied diameter, straightness and cut length before machining. See bright bar finishes for related options.
Solution annealing and controlled cooling help maintain the intended ferrite-austenite balance. Incorrect thermal processing may allow unwanted phases that reduce toughness and corrosion resistance. The required delivery condition should match the product specification and service application.
Keep the heat number with each bar and cut piece throughout storage and machining. Match the mill test certificate to the UNS S31803 grade, chemistry, mechanical results and purchase order. Additional corrosion or microstructure testing may be needed for critical projects. See quality assurance information.
Frequently asked questions
UNS S31803 is a duplex stainless steel containing ferrite and austenite. It offers high strength and corrosion resistance for suitable chemical, marine and industrial conditions.
They belong to the duplex 2205 family but have different chemistry ranges. S32205 specifies tighter chromium, molybdenum and nitrogen limits. Check the UNS grade required by the drawing and certificate.
ASTM A276/A276M covers stainless steel bars and shapes, while ASTM A479/A479M may apply to pressure-service bars. Confirm that the chosen grade and condition are covered in the specified edition.
Yes. Its ferrite phase normally gives duplex S31803 a magnetic response, even when properly solution annealed.
Yes. Because of the grade's high strength, suitable tooling, cutting speeds and secure workholding are important. Specify the finished diameter and tolerance before ordering.
Correct heat treatment and cooling help provide the intended duplex microstructure. Poorly controlled processing can reduce corrosion resistance and toughness.
Keep the bars dry, supported and separated from carbon steel dust and grinding debris. Preserve heat numbers and labels so every cut piece remains traceable to its material certificate.
Related products
Specification-led enquiries
Include the governing standard, dimensions, quantity, condition, testing requirements, documentation, and destination.